BS EN 10025-3:2019 pdf free.Hot rolled products of structural steels. 7.3.1.1 Under the inspection and testing conditions, as specified in Clauses8, 9 and 10, and in the .delivery condition, as specified in 6.3,as well as after normalizing heat treatment after delivery (including delayed cooling or tempering if needed for steels with a minimum yield strength 2 420 MPa) the mechanical...